- Source: Nickel sulfide
Nickel sulfide is any inorganic compound with the formula NixSy. These compounds range in color from bronze (Ni3S2) to black (NiS2). The nickel sulfide with simplest stoichiometry is NiS, also known as the mineral millerite. From the economic perspective, Ni9S8, the mineral pentlandite, is the chief source of mined nickel. Other minerals include heazlewoodite (Ni3S2) and polydymite (Ni3S4), and the mineral Vaesite (NiS2). Some nickel sulfides are used commercially as catalysts.
Structure
Like many related materials, nickel sulfide adopts the nickel arsenide motif. In this structure, nickel is octahedral and the sulfide centers are in trigonal prismatic sites.
NiS has two polymorphs. The α-phase has a hexagonal unit cell, while the β-phase has a rhombohedral cell. The α-phase is stable at temperatures above 379 °C (714 °F), and converts into the β-phase at lower temperatures. That phase transition causes an increase in volume by 2–4%.
Synthesis and reactions
The precipitation of solid black nickel sulfide is a mainstay of traditional qualitative inorganic analysis schemes, which begins with the separation of metals on the basis of the solubility of their sulfides. Such reactions are written:
Ni2+ + H2S → NiS + 2 H+
Many other more controlled methods have been developed, including solid state metathesis reactions (from NiCl2 and Na2S) and high temperature reactions of the elements.
The most commonly practiced reaction of nickel sulfides involves conversion to nickel oxides. This conversion involves heating the sulfide ores in air:
NiS + 1.5 O2 → NiO + SO2
Occurrence
= Natural
=The mineral millerite is also a nickel sulfide with the molecular formula NiS, although its structure differs from synthetic stoichiometric NiS due to the conditions under which it forms. It occurs naturally in low temperature hydrothermal systems, in cavities of carbonate rocks, and as a byproduct of other nickel minerals.
In nature, nickel sulfides commonly occur as solid solutions with iron sulfides in minerals such as pentlandite and pyrrhotite. These minerals have the formula Fe9-xNixS8 and Fe7-xNixS6, respectively. In some cases they are high in nickel (larger values of x).
= In glass manufacturing
=Float glass contains a small amount of nickel sulfide, formed from the sulfur in the fining agent Na2SO4 and the nickel contained in metallic alloy contaminants.
Nickel sulfide inclusions are a problem for tempered glass applications. After the tempering process, nickel sulfide inclusions are in the metastable alpha phase. The inclusions eventually convert to the beta phase (stable at low temperature), increasing in volume and causing cracks in the glass. In the middle of tempered glass, the material is under tension, which causes the cracks to propagate and leads to spontaneous glass fracture. That spontaneous fracture occurs years or decades after glass manufacturing.
References
Kata Kunci Pencarian:
- Nikel sulfida
- Parvathi Basrur
- Paladium
- Seng
- Tembaga
- Hidrogen
- Belerang
- Galium
- Kamus rumus kimia
- Nonlogam
- Nickel sulfide
- Cobalt extraction
- Sulfide
- Pentlandite
- Nickel sulfide inclusion
- Ore genesis
- Nickel
- Sulfide mineral
- Nickel mine
- Millerite